Discuss a project →
Guides

Integrated security glazing: forced entry, ballistic, blast and fire

Combined fire, forced-entry, ballistic and blast performance in a single assembly Combined fire, forced-entry, ballistic and blast performance in a.

Combined fire, forced-entry, ballistic and blast performance in a single assembly Combined fire, forced-entry, ballistic and blast performance in a single assembly A window asked to resist fire, forced entry, gunfire and blast is not four products stacked together. It is one assembly that must satisfy four unrelated test regimes simultaneously — and the measures that satisfy one routinely degrade another.

This guide sets out the four performance families, the standards that govern each, and — most importantly — the interaction effects that determine whether a specified combination is buildable at all.

The four families, and why they do not add up

Each family is defined by a different physical event, measured by a different test, and expressed in a different vocabulary. There is no common unit and no conversion between them.

A build-up certified to one family carries no standing in another. Ballistic certification implies nothing about blast; blast certification implies nothing about fire; and none of them implies forced-entry resistance. Each has to be evidenced separately, and each has to be evidenced for the same physical assembly — the same glass, interlayer, frame, bite, gasket, hardware and fixing.

Forced entry

Forced-entry resistance is a time standard, not a strength standard. The assembly is attacked by trained operatives with a defined tool set for a defined period; it passes if no man-passable opening is created within that period. Glass that breaks but does not open is a pass.

By class, reflecting the tool set and attack duration. Lower classes address basic hand tools; higher classes address heavy hand tools sustained over several minutes HPW-TP-0500.0 US Department of State physical security test protocol, applied to diplomatic and mission entry-control glazing By level, generally aligned to a stated attack duration SD-STD-01.01 US Department of State forced entry and ballistic standard for certified protective glazing Commonly quoted at 5, 15 and 60-minute forced-entry durations ASTM F3561 Newer standard addressing combined forced entry and ballistic attack Sequential ballistic attack followed by forced-entry attack on the weakened assembly The consequence for glass make-up. Forced-entry resistance at the higher classes cannot be achieved with conventional polyvinyl butyral. Standard PVB is ductile and tears progressively under repeated tool strikes. Ionoplast interlayers — SentryGlas and equivalents — are approximately two orders of magnitude stiffer at room temperature and retain post-breakage structural capacity, which is why they are specified as mandatory above the lower classes. Polycarbonate composite strike faces are an alternative, at a cost in optical quality, abrasion resistance and thickness.

Forced-entry duration is the parameter most often omitted from a specification. “Class III” without a stated attack time, tool set and reference protocol cannot be procured or verified, because the classes in the architectural and diplomatic standards are not interchangeable.

Ballistic

BR classes under EN 1063 apply to the glazing alone, tested as a 500 × 500 mm specimen. FB classes under EN 1522 and EN 1523 apply to the complete assembly including frame, seals, hinges and fixings. BR7 glazing in an untested frame is not an FB7 window — a round that cannot pass through the glass will pass through a bead, a gasket line or a fixing that was never tested.

3.3 Spall — the criterion that decides where people can stand A build-up may stop the projectile and still eject fragments from the protected face at velocities capable of causing serious injury. EN 1063 records this as a suffix: NS where no splinters are released, S where they are. UL 752 requires no spall at the ratings it grants. NIJ 0108.01 does not assess spall at all, which is a material limitation when that standard is cited for occupied positions.

  • Canting the glazing from vertical, typically by around ten degrees, so that a round strikes obliquely and any spall is directed away from the operator. This is a frame and architectural decision that must be taken at design stage, not at shop drawing stage.
  • An anti-spall film on the protected face, typically 350 micron. Effective, but it becomes part of the tested assembly and cannot simply be added to a certified build-up without re-establishing the classification.

Blast

Blast is the only one of the four families where the specification routinely fails to define the demand at all. A hazard rating states the acceptable outcome; it does not state the load. Both are required.

4.1 Defining the load A blast load is described by peak reflected overpressure, positive phase duration and reflected impulse. Idealising the decay as linear, ir ≈ ½ · Pr · td, so any two define the third. Which parameter governs the response depends on the ratio of load duration to the natural period of the glazing, which for architectural panes is typically in the region of ten to thirty milliseconds.

Incident or reflected must be stated. A free-field side-on gauge and the building face read different pressures. At the low overpressures typical of process facility design the reflection factor is approximately two, rising sharply with pressure. A specification that gives a pressure without declaring which it is, is at minimum a factor of two ambiguous — and that ambiguity propagates through glass selection, frame sizing, anchorage design and structural verification.

4.2 Defining the acceptable outcome GSA-TS01-2003 measures outcome by where the glass lands relative to a witness panel three metres behind the opening. The distinction between Condition 2 and Condition 3 is fundamental: Condition 2 requires the glazing to be retained by the frame; Condition 3 permits failure and controls only the travel distance.

The cost difference between Condition 2 and Condition 3a is substantial and structural. Retention in the frame demands greater bite depth, a stiffer frame section, engineered anchorage in both directions and, frequently, structural silicone at every bonding line. Where a specification cites a Condition number alongside a descriptive text, and the two do not correspond, this must be resolved before any assembly is selected.

Suffix NS denotes no splinters detached from the protected face; S permits splintering. EN 13123 and EN 13124 extend classification to complete windows, doors and shutters — EPR classes by shock tube, EXR classes by open range test. ISO 16933 provides open-arena classification with EXV vehicle-bomb and SB satchel-bomb classes; ISO 16934 the shock tube equivalent.

None of these systems converts into any other. An EN 13541 ER2 classification carries no GSA Performance Condition and no ASTM hazard rating, and the reverse holds equally. Where a project cites more than one system, each must be evidenced independently for the assembly as supplied.

Fire

European classification to EN 13501-2 uses three criteria, each with a period in minutes: E integrity, the exclusion of flame and hot gases; W radiation, limiting radiated heat on the unexposed face; I insulation, limiting temperature rise on the unexposed face. The subscripts EI1 and EI2, applicable to doorsets only, differ in the location of temperature measurement relative to the frame and glazing edge.

North American practice divides fire-rated glazing into fire-protective products, tested to NFPA 252 / UL 10C and NFPA 257 / UL 9, which exclude flame and smoke but not radiant heat and are therefore subject to area limitation; and fire-resistive products, tested to ASTM E119, UL 263 or NFPA 251 to the same criteria as a wall, and consequently not area-limited. Assemblies rated above 20 minutes must additionally survive the hose stream test.

The functional distinction is between excluding flame and excluding heat. It maps loosely onto the E and EI classes but is not an equivalence: the furnace curves, pass criteria and hose stream requirement differ, and a product classified under one system holds no standing under the other.

Interaction effects

This is where combined-performance specifications succeed or fail. The measures that satisfy one performance family frequently degrade another, and several combinations that appear reasonable on paper are not buildable as certified assemblies.

6.1 Fire and ballistic are largely mutually exclusive Insulating fire-rated glazing achieves its EI performance through intumescent interlayers that expand and opacify under heat. These layers are formulated for thermal behaviour, not structural capacity; they are not ballistic interlayers and cannot be substituted for one. Conversely, a ballistic build-up of thick glass plies and ionoplast interlayers has no fire classification and will fail an integrity test rapidly. Products combining both exist, but they are specific certified constructions — not a matter of adding plies. Where a single opening is required to be both fire and ballistic rated, this must be identified at design stage, because the available product set is narrow and the lead times are long.

  • Annealed float fractures into large, sharp shards. It is the worst performer under blast and should not appear on the protected face of any security assembly.
  • Fully tempered is substantially stronger and dices on failure, but releases the entire pane at once and stores significant strain energy — under blast the failure is sudden and total.
  • Heat-strengthened offers intermediate strength with a larger fracture pattern that laminates hold together more effectively. It is frequently the preferred substrate for laminated blast glazing for precisely this reason.
  • Laminated construction is what actually delivers retention. The glass carries load until it breaks; the interlayer carries it thereafter.

6.4 Insulating unit orientation In an insulating glass unit the outer lite is effectively sacrificial under blast: it fails first and its fragments are ejected outwards. The inner lite governs what enters the occupied space. Placing the laminated security build-up on the outer position and a monolithic pane on the inner position therefore inverts the intended protection — the laminate absorbs energy the occupant never sees, while the unlaminated inner pane becomes the fragment source.

Where an insulating unit is required for thermal reasons in a blast-rated zone, the security laminate belongs on the inboard lite. Where a specification shows the reverse, it should be queried before procurement. Where thermal performance is not required — internal partitions, screening counters, gatehouse vision panels — a monolithic laminate is both better performing and considerably less expensive than an insulating unit.

6.5 Thermal stress in Gulf service Thick multi-ply laminates absorb substantially more solar energy than conventional glazing. Combined with high ambient temperatures, partial shading from deep reveals or canopies, internal blinds close to the glass, and any solar-control coating, the resulting temperature differential across a pane can exceed the thermal stress capacity of annealed glass. Any annealed component in a security build-up should be assessed for thermal stress, and heat-strengthening specified where the assessment requires it. This is a routine cause of unexplained glass breakage in the region and it is unrelated to the security performance.

6.6 The weight cascade Soda-lime glass masses approximately 2.5 kg per square metre per millimetre of thickness. A combined forced-entry, ballistic and blast build-up of the order of 40 mm of glass, plus interlayers, approaches 100 kg/m². A single unit at 1.5 × 2.5 m therefore approaches 375 kg.

Frame, bite and anchorage

In published blast trials the recorded failures are overwhelmingly failures of the frame, the fixings and the adhesive bonds — not of the glass. The load must travel from the glass surface through the bite, the gasket, the bead or pressure plate, the frame section, the anchor and into the structure, and it will find the weakest element on that path.

  • Bite depth governs whether the pane can pull out of the rebate before the glazing has developed its capacity. Higher performance levels demand deeper bite, which increases frame depth and reduces vision area — an architectural consequence that must be resolved early.
  • Edge cover and setting blocks determine how load is introduced into the glass edge. Concentrated bearing at the corners initiates failure well below the theoretical capacity.
  • Reversal. The negative phase of a blast reverses the reaction at every fixing. Details that bear only in compression release the glazing on rebound. This is a documented failure mode, not a theoretical one.
  • Anchorage reactions must be calculated, stated and issued to the project structural engineer for verification of the receiving structure. A correctly engineered window fixed into inadequate construction is not a rated installation.
  • Structural sealant grade and cure regime form part of the certified assembly. Single and two-component silicones are not interchangeable where the specification distinguishes them, and full cure periods are measured in weeks, not days — a programme item, not a detail.

Test evidence, and what invalidates it

  • A report attests to the specimen tested. Any material departure — glass make-up, interlayer, overall size, aspect ratio, frame section, bite, fixing centres or the addition of an applied film — places the installed configuration outside the tested envelope. A tested product installed to an untested detail is an uncertified product, and extension beyond the tested envelope requires documented engineering justification, declared on the submittal.

Capability

  • In-house design office — structural calculation, thermal and acoustic modelling, blast assembly engineering and bespoke detail development. Every project is engineered as a complete frame, glass and hardware assembly.
  • Controlled standards library — American and European fire, forced-entry, ballistic and blast standards, so design work begins from the correct performance criteria rather than from an assumption.
  • Accredited third-party testing — products are developed towards, and validated by, independent test at accredited laboratories, with the tested configuration fully recorded.
  • Certified detail discipline — the tested detail is treated as fixed. Any proposed departure is handled as a formal deviation and disclosed, not absorbed silently into the shop drawings.

How to start. Issue the elevations, the door and window schedule with type tags, the compartmentation and security zoning drawings, and whatever performance criteria have been established. Where the criteria are incomplete — and in combined-performance packages they usually are — we will set out precisely what is missing, what we have assumed in the interim, and what the assumption is worth in cost terms, before anything is priced.

Issued for information. Selection of fire ratings, forced-entry classes, ballistic levels, design blast loads and hazard ratings is the responsibility of the project's fire engineer, security consultant, blast engineer and the authority having jurisdiction. This document does not constitute fire, security or blast engineering advice. Threat data and classification descriptions are summarised for guidance; classification for any assembly is established solely by test to the governing standard. Standards are cited as at the date shown and this guide is revised without notice; always work from the current issue.

The full guide

This page gives the text of our technical guide. The tables, charts and quick-reference sheet are in the PDF: download the full guide.

Related

Have a project requirement?

Send your drawings, specification and project location. Tell us what the opening needs to achieve and where you need support.